Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.02 g/cc | 0.109 lb/in³ | |
PCC-Advanced Forming Technology AlSiC-SD Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Density | 3.02 g/cc | 0.109 lb/in³ | |
Ferro EG 2810 Dental Glass Glass Type: Ba-Al-B-Si Typical Application: Glass Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also manufacture.. |
|||
Density | 3.02 g/cc | 0.109 lb/in³ | ASTM C135 |
M Cubed Technologies HSC-702 Aluminum-toughened Reaction Bonded Silicon Carbide High fracture tougness reaction bonded SiC. Used in applications that require both high wear and high impact resistance. Bullnoses, fan liners, hydrocyclone liners, etc.Information provided by M C.. |
|||
Density | 3.02 g/cc | 0.109 lb/in³ | |
Ceradyne Ceralloy® 2710 BeO-SiC Applications:terminationssever wedgesload pelletsabsorbersFeatures: former industry standard for terminations etc.Information provided by Ceradyne Company |