Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 2.27 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.19 - 2.27 g/cc
0.0791 - 0.0820 lb/in³
BS2782:Pt6
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
Density 2.19 - 2.27 g/cc
0.0791 - 0.0820 lb/in³
BS2782:Pt6
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..
Density 2.19 - 2.27 g/cc
0.0791 - 0.0820 lb/in³
BS2782:Pt6
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
Density 2.19 - 2.27 g/cc
0.0791 - 0.0820 lb/in³
BS2782:Pt6
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..
Density 2.07 - 2.27 g/cc
0.0748 - 0.0820 lb/in³
Molded
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester
BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig..