Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.19 - 2.27 g/cc | 0.0791 - 0.0820 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Density | 2.19 - 2.27 g/cc | 0.0791 - 0.0820 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Density | 2.19 - 2.27 g/cc | 0.0791 - 0.0820 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Density | 2.19 - 2.27 g/cc | 0.0791 - 0.0820 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Density | 2.07 - 2.27 g/cc | 0.0748 - 0.0820 lb/in³ | Molded |
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig.. |