Physical Properties Metric English Comments
Density >= 14.0 g/cc
>= 0.506 lb/in³
Hogen Duralloy H5W 70 Tungsten/30 Copper PM Metal Composite
RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is ..
Density >= 14.0 g/cc
>= 0.506 lb/in³
Mi-Tech Metals CW70 70 Tungsten/30 Copper PM Metal Composite
RWMA Class 10.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recomme..
Density 14.0 g/cc
0.506 lb/in³
Wieland 1403 Wilaform Gold
Hard yellow gold alloy. Universally applicable in decoration production. Since it does not posses a very fine-grained structure it is used frequently for chainsApplications: casting, chains, lamin..
Density 14.0 - 14.5 g/cc
0.506 - 0.524 lb/in³
China Tungsten YG11C Cemented Tungsten Carbide for Mining Purposes
For tipping of bits for heavy rock drills and rotary hammer rock drills cutting hard rock formations . e. g. , latent hole drills and deep-hole drills, rock drills, etc.Information provided by China..
Density 14.0 - 14.3 g/cc
0.506 - 0.517 lb/in³
China Tungsten YG13C Cemented Tungsten Carbide for Mining Purposes
For oil cone drills, for hard and medium hard rock and for tipping bit of rotary hammer rock drills and heavy rock drills.Information provided by China Tungsten
Density 14.0 g/cc
0.506 lb/in³
China Tungsten YG15 Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.0 g/cc
0.506 lb/in³
China Tungsten YG15C Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.0 g/cc
0.506 lb/in³
China Tungsten YG15X Tungsten Carbide Powder
Information provided by China Tungsten