Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.1 - 14.5 g/cc | 0.509 - 0.524 lb/in³ | |
H.C. Starck WCu 70/30 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
Density | 14.0 - 14.5 g/cc | 0.506 - 0.524 lb/in³ | |
China Tungsten YG11C Cemented Tungsten Carbide for Mining Purposes For tipping of bits for heavy rock drills and rotary hammer rock drills cutting hard rock formations . e. g. , latent hole drills and deep-hole drills, rock drills, etc.Information provided by China.. |