Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 13.5 - 14.7 g/cc | 0.488 - 0.531 lb/in³ | |
China Tungsten YT6S Tungsten Carbide Having the same wear resistance as YG6X but higher toughness. for tobacco cutters and rough and finish milling of cast iron.Information provided by China Tungsten |
|||
Density | 13.5 g/cc | 0.488 lb/in³ | |
China Tungsten ZM30 Tungsten Carbide High strength in use; capable of resisting high impact load, yet wear resistance comparatively low. Roughing and semi-finishing of refractory steel, manganese steel, stainless steel, etcInformation.. |