China Tungsten ZM30 Tungsten Carbide

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten ZM30 Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High strength in use; capable of resisting high impact load, yet wear resistance comparatively low. Roughing and semi-finishing of refractory steel, manganese steel, stainless steel, etcInformation provided by China Tungsten
Physical Properties Metric English Comments
Density 13.5 g/cc
0.488 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 90.5
90.5
Flexural Strength 2000 MPa
290000 psi