China Tungsten YT6S Tungsten Carbide

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YT6S Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Having the same wear resistance as YG6X but higher toughness. for tobacco cutters and rough and finish milling of cast iron.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 13.5 - 14.7 g/cc
0.488 - 0.531 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 91
91
Flexural Strength 1500 MPa
218000 psi