Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.14 - 1.97 g/cc | 0.0412 - 0.0712 lb/in³ | Average value: 1.56 g/cc Grade Count:324 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Density | 0.927 - 1.97 g/cc | 0.0335 - 0.0711 lb/in³ | Average value: 1.20 g/cc Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade". Each property range of values reported is min.. |