Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.927 - 1.97 g/cc
0.0335 - 0.0711 lb/in³
Average value: 1.20 g/cc Grade Count:4
Vinyl Acetate Content 17.9 - 40.0 %
17.9 - 40.0 %
Average value: 32.6 % Grade Count:3
Melt Flow 2.10 - 6.00 g/10 min
2.10 - 6.00 g/10 min
Average value: 3.78 g/10 min Grade Count:5
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.80 - 11.7 MPa
1420 - 1700 psi
Average value: 10.9 MPa Grade Count:4
Elongation at Break 750 - 981 %
750 - 981 %
Average value: 865 % Grade Count:4
Users viewing this material also viewed the following: