Parylene Coating Services D Poly (P-Xylylene)

Category Polymer , Thermoplastic , Poly (P-Xylylene)
Manufacturer Parylene Coating Services, Inc. (PCS)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parylene Coating Services D Poly (P-Xylylene).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Monomer is dichloro para-xylylene. Parylene D is recommended where high temperature resistance is needed; it can be used up to 140°C where oxygen is present.Parylene is a generic name for poly-para-xylylene polymers used as conformal coatings in protective applications.The coating process exposes objects to the gas-phase monomer at low pressure. Through vacuum deposition, Parylene condenses on the surface in a polycrystalline fashion, providing a coating that is truly conformal and pinhole free.Compared to liquid processes, the effects of gravity and surface tension are negligible -- so there is no bridging, thin-out, pinholes, puddling, run-off or sagging. And, since the process takes place at room temperature, there is no thermal or mechanical stress on the object.Parylene is physically stable and chemically inert within its usable temperature range. Parylene provides excellent protection from moisture, salt spray, corrosive vapors, solvents, airborne contaminants and other hostile environments.Property data obtained following ASTM methods. Information provided by Parylene Coating Services, Inc. (PCS)
Physical Properties Metric English Comments
Density 1.418 g/cc
0.05123 lb/in³
Moisture Vapor Transmission 0.0984 cc-mm/m²-24hr-atm
0.250 cc-mil/100 in²-24hr-atm
37°C; 90% RH
Oxygen Transmission 12.6 cc-mm/m²-24hr-atm
32.0 cc-mil/100 in²-24hr-atm
23°C
Nitrogen Transmission 1.77 cc-mm/m²-24hr-atm
4.50 cc-mil/100 in²-24hr-atm
23°C
Carbon Dioxide Transmission 5.12 cc-mm/m²-24hr-atm
13.0 cc-mil/100 in²-24hr-atm
23°C
Hydrogen Sulfide Transmission 0.571 cc-mm/m²-24hr-atm
1.45 cc-mil/100 in²-24hr-atm
23°C
Sulfur Dioxide Transmission 1.87 cc-mm/m²-24hr-atm
4.75 cc-mil/100 in²-24hr-atm
23°C
Chlorine Transmission 0.217 cc-mm/m²-24hr-atm
0.550 cc-mil/100 in²-24hr-atm
23°C
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.8 MPa
11000 psi
Tensile Strength, Yield 62.1 MPa
9000 psi
Elongation at Break 10 %
10 %
Elongation at Yield 3.0 %
3.0 %
Tensile Modulus 2.80 GPa
406 ksi
Coefficient of Friction, Dynamic 0.31
0.31
Coefficient of Friction, Static 0.33
0.33
Thermal Properties Metric English Comments
Melting Point 380 °C
716 °F
Maximum Service Temperature, Air 140 °C
284 °F
Optical Properties Metric English Comments
Refractive Index 1.669
1.669
Transmission, Visible 90 %
90 %
Optically clear, but reports do not quantify.
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+16 ohm-cm
2.00e+16 ohm-cm
50% RH
Surface Resistance 5.00e+16 ohm
5.00e+16 ohm
50% RH
Dielectric Constant 2.8

@Frequency 1e+6 Hz
2.8

@Frequency 1e+6 Hz
2.84

@Frequency 60 Hz
2.84

@Frequency 60 Hz
2.95

@Frequency 1000 Hz
2.95

@Frequency 1000 Hz
Dielectric Strength 217 kV/mm
5500 kV/in
Short Time; 1 mil
Dissipation Factor 0.0020

@Frequency 1e+6 Hz
0.0020

@Frequency 1e+6 Hz
0.0030

@Frequency 1000 Hz
0.0030

@Frequency 1000 Hz
0.0040

@Frequency 60 Hz
0.0040

@Frequency 60 Hz
Users viewing this material also viewed the following: