Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.115 g/cc | 0.04028 lb/in³ | ISO 1183 |
Lanxess Durethan® DP BC 310 EF 000000 Nylon 6 PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow) |
|||
Density | 1.115 g/cc | 0.04028 lb/in³ | ISO 1183 |
Stir SpA CT 33 ATC (PVC) Application: Suction cupsInformation provided by STIR SpA |
|||
Density | 1.115 g/cc | 0.04028 lb/in³ | |
BASF N-Acetylmorpholine Formula: C6H11NO2CAS: 1696-20-4Description: N-Acetylmorpholine is a colorless to yellowish liquid, with a faint odor. It is fully soluble with water.Synonyms: AcetomorpholideApplications: Intermedia.. |