Polymer Property : Density = 0.04028 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.115 g/cc
0.04028 lb/in³
ISO 1183
Lanxess Durethan® DP BC 310 EF 000000 Nylon 6
PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow)
Density 1.115 g/cc
0.04028 lb/in³
ISO 1183
Stir SpA CT 33 ATC (PVC)
Application: Suction cupsInformation provided by STIR SpA
Density 1.115 g/cc
0.04028 lb/in³
BASF N-Acetylmorpholine
Formula: C6H11NO2CAS: 1696-20-4Description: N-Acetylmorpholine is a colorless to yellowish liquid, with a faint odor. It is fully soluble with water.Synonyms: AcetomorpholideApplications: Intermedia..