Density 0.9586 - 1.0185 g/cc
0.03463 - 0.036796 lb/in³
Lord Adhesives Flocklok® 855 Flock Adhesive
LORD Flocklok® 855 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good res..