Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9586 - 1.0185 g/cc | 0.03463 - 0.036796 lb/in³ | |
Lord Adhesives Flocklok® 855 Flock Adhesive LORD Flocklok® 855 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good res.. |