Lord Adhesives Flocklok® 855 Flock Adhesive

Category Polymer , Adhesive
Manufacturer Lord Adhesives
Trade Name Flocklok®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Flocklok® 855 Flock Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LORD Flocklok® 855 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good resistance to abrasion. Flocklok 855 flock adhesive will react and cure with moisture; however, an elevated temperature cure is required to optimize adhesion and performance properties.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.9586 - 1.0185 g/cc
0.03463 - 0.036796 lb/in³
Solids Content 49 - 54 %
49 - 54 %
Viscosity 40 - 275 cP

@Temperature 25.0 °C
40 - 275 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point 19.0 °C
66.2 °F
Seta
Processing Properties Metric English Comments
Cure Time 2.00 min

@Temperature 232 °C
0.0333 hour

@Temperature 450 °F
2.50 min

@Temperature 204 °C
0.0417 hour

@Temperature 399 °F
Descriptive Properties Value Comments
Appearance Brown Liquid
Solvents Xylene, MIBK, Acetates