Polymer Property : Density = 0.8747 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.850 - 0.8747 g/cc
0.0307 - 0.03160 lb/in³
Chemlok® 485
Lord Adhesives Chemlok® 485/Curative 44 Adhesive
LORD Chemlok® 485/Curative 44 adhesive is a two component adhesive system used for insert mold bonding of PVC and Alcryn® to substrates such as metal, rubber and other thermoplastic elastomers..