BASF Pentanol

Category Fluid , Solvent
Manufacturer BASF
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pentanol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formula: C5H12OCAS: 71-41-0Description: Pentanol is a colorless liquid with an offensive odor.Synonyms: Pentan-1-ol, 1-Pentanol, n-Amyl alcoholApplications: Intermediate used in the production of Corrosion inhibitors, Flotation aids, Pharmaceuticals, Lubricating oil additives, Herbicides, Cosmetics, Antioxidants, Extractants, Essences and paint solvents and StabilizersInformation provided by BASF
Physical Properties Metric English Comments
Density 0.815 g/cc
0.0294 lb/in³
Molecular Weight 88.2 g/mol
88.2 g/mol
Thermal Properties Metric English Comments
Melting Point <= -70.0 °C
<= -94.0 °F
Boiling Point 137 - 139 °C
279 - 282 °F
Flash Point 49.0 °C
120 °F
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
DIN 51 777
Descriptive Properties Value Comments
Assay >98.5%
Ignition Temperature 300°C