Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.736 g/cc @Temperature 15.0 °C |
0.0266 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Exxsol™ DSP100/120 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.736 g/cc | 0.0266 lb/in³ | |
Pyrotek E-1 Board Structural Insulating Board E-1 is a high-temperature board designed to combine structural strength and high insulating value. Structural insulation panels made from E-1 can be painted. Fibers generated while cutting E-1 are .. |