Pyrotek E-1 Board Structural Insulating Board

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek E-1 Board Structural Insulating Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
E-1 is a high-temperature board designed to combine structural strength and high insulating value. Structural insulation panels made from E-1 can be painted. Fibers generated while cutting E-1 are classified by OSHA as nuisance dust only.ApplicationsStructural insulation panels Furnace insulation Machined parts AdvantagesStrong light weight material Easily cut and machined Economical Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.736 g/cc
0.0266 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.380 MPa
55.1 psi
across grain
1.39 MPa
202 psi
with grain
Shear Strength 0.690 MPa
100 psi
across grain
2.79 MPa
405 psi
with grain
Thermal Properties Metric English Comments
Thermal Conductivity 0.124 W/m-K

@Temperature 538 °C
0.861 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Maximum Service Temperature, Air 704 °C
1300 °F
Continuous use
1093 °C
1999 °F