Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.737 - 0.865 g/cc | 0.0266 - 0.0313 lb/in³ | |
Pyrotek SF-50 Foamed Fused Silica Insulation Board SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o.. |
|||
Density | 0.737 g/cc | 0.0266 lb/in³ | |
Trelleborg AEM Syntac® Eccolite® Ultra Eccolite® Ultra is a new generation syntactic foam plug assist material, a new thermoplastic compound developed in response to the needs of the thermoforming industry. Eccolite® is tough and robus.. |
|||
Density | 0.736 g/cc @Temperature 15.0 °C |
0.0266 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Exxsol™ DSP100/120 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.737 g/cc | 0.0266 lb/in³ | |
CMT Materials HYTAC® C1R Highly Durable Syntactic Foam, Dust-Free Machining/Polishing HYTAC-C1R is easily machined without the dust typically associated with epoxy syntactic foam. This new copolymer base has been optimized for both the machine shop and the thermoforming process.Exce.. |
|||
Density | 0.737 g/cc | 0.0266 lb/in³ | ASTM C134 |
BNZ Materials C-22 Z Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.737 g/cc | 0.0266 lb/in³ | |
BNZ Materials Marinite® I&M High Temperature Structural Insulation Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating.. |
|||
Density | 0.737 g/cc | 0.0266 lb/in³ | |
Trelleborg AEM Syntac® 450 Syntactic Foam Syntac® 450 syntactic foam is the high temperature (450°F/232°C) member of the Syntac® product family.A rigid, high strength composite of epoxy resin and hollow glass microspheres, Syntac® 450 .. |
|||
Density | 0.736 g/cc | 0.0266 lb/in³ | |
Pyrotek E-1 Board Structural Insulating Board E-1 is a high-temperature board designed to combine structural strength and high insulating value. Structural insulation panels made from E-1 can be painted. Fibers generated while cutting E-1 are .. |