Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.5 - 15.0 g/cc | 0.524 - 0.542 lb/in³ | |
MarkeTech WCu25 Tungsten Copper Alloy Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Density | 14.6 - 15.0 g/cc | 0.527 - 0.542 lb/in³ | |
China Tungsten YG6 Cemented Tungsten Carbide for Mining Purposes For coring crowns, electric coal drill bits, coal cutting picks. oil cone bits and scraping knife bits used in geological prospecting, coal mining and oil well boringInformation provided by China Tu.. |
|||
Density | 14.6 - 15.0 g/cc | 0.527 - 0.542 lb/in³ | |
China Tungsten YG6 Tungsten Carbide for Dies and Wear Part Making For drawing of steels, non-ferrous metal and alloy bars of |
|||
Density | 14.6 - 15.0 g/cc | 0.527 - 0.542 lb/in³ | |
China Tungsten YG6X Tungsten Carbide for Dies and Wear Part Making For drawing of steel wires and non-ferrous metal wires or bars of |
|||
Density | 14.85 - 15.0 g/cc | 0.5365 - 0.542 lb/in³ | |
China Tungsten Z10 Tungsten Carbide for Mining Purposes High wear resistance, for pillar bit drills.Information provided by China Tungsten |