Polymer Property : Density = 0.5365 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 14.85 g/cc
0.5365 lb/in³
China Tungsten YG6X Tungsten Carbide
Information provided by China Tungsten
Density 14.85 - 15.0 g/cc
0.5365 - 0.542 lb/in³
China Tungsten Z10 Tungsten Carbide for Mining Purposes
High wear resistance, for pillar bit drills.Information provided by China Tungsten