Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.346 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 9.58 g/cc
0.346 lb/in³
Indium Corp. Indalloy 40 Bismuth Solder Alloy
Information Provided by Indium Corporation
Density 9.59 g/cc
0.346 lb/in³
Indium Corp. Indalloy 50 Bismuth Solder Alloy
Information Provided by Indium Corporation
Density 9.58 g/cc
0.346 lb/in³
Indium Corp. Indalloy 99 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Density 9.59 g/cc
0.346 lb/in³
Indium Corp. Indalloy 24 Bismuth Solder Alloy
Information Provided by Indium Corporation
Density 9.58 g/cc
0.346 lb/in³
Indium Corp. Indalloy® 158 Bi-Pb-Sn-Cd Solder Alloy
Lowest melting point solder. Good fusible alloy used for lens blocking.Information provided by the manufacturer, Indium Corporation.
Density 9.58 g/cc
0.346 lb/in³
Williams Advanced Alloys WS96 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 9.59 g/cc
0.346 lb/in³
CMW® D55 Silver Cadmium Oxide Contact Material ASTM B781, Table 2, Type B
For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc.
Density 9.58 g/cc
0.346 lb/in³
Indium Corp. Indalloy 214 Silver Solder Alloy
Information Provided by Indium Corporation
Copyright © lookpolymers.com All Rights Reserved