Physical Properties Metric English Comments
Density 6.68 g/cc
0.241 lb/in³
Ferro CF 7567 Low-Temperature Sealing
VITREOUS Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific therm..
Density 6.67 g/cc
0.241 lb/in³
Sintered
Ametek P409L P/M Stainless Steel, Sintered from 6.60 g/cc Green Density
P409L is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and ha..
Density 6.68 g/cc
0.241 lb/in³
Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.65 g/cc Green Density
Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i..
Density 6.68 g/cc
0.241 lb/in³
Ametek Ultra 304L P/M Stainless Steel, Sintered from 6.75 g/cc Green Density
Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i..
Density 6.67 g/cc
0.241 lb/in³
Sintered
Ametek P409L/409CB P/M Stainless Steel, Sintered from 6.60 g/cc Green Density
P409L/409CB is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance ..
Density 6.67 g/cc
0.241 lb/in³
Ametek P410L P/M Stainless Steel, Sintered from 6.6 g/cc Green Density
Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for ..