Ametek Ultra 304L P/M Stainless Steel, Sintered from 6.75 g/cc Green Density

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Ametek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ametek Ultra 304L P/M Stainless Steel, Sintered from 6.75 g/cc Green Density.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement in corrosion resistance, while other properties are comparable to the conventional counterparts.Mechanical property data below is from samples lubricated with 1% Acrawax C and pressed at 50 tsi. Green strength 1200 ksi. Specimens were delubricated in air for 20 min. at 950°F (510°C), then sintered in dissociated ammonia for 30 min. at 2100°F (1149°C) and cooled in the water jacketed furnace cooling zone. Dimensional change from die size -0.0%.Information provided by Ametek Specialty Metal Products.
Physical Properties Metric English Comments
Density 6.68 g/cc
0.241 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 62
62
Tensile Strength, Ultimate 340 MPa
49300 psi
Tensile Strength, Yield 270 MPa
39200 psi
Elongation at Break 4.8 %
4.8 %
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 19 %
19 %
Copper, Cu 0.80 %
0.80 %
Iron, Fe 66 %
66 %
as balance
Manganese, Mn 0.20 %
0.20 %
Nickel, Ni 11 %
11 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.80 %
0.80 %
Sulfur, S 0.010 %
0.010 %
Tin, Sn 2.0 %
2.0 %