MarkeTech Zirconium Oxide Ceramic, Zirconia MgO Stabilized

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer MarkeTech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Zirconium Oxide Ceramic, Zirconia MgO Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is significantly improved. This makes some grades of zirconia superior to most materials for abrasion and wear resistance. Parts can be machined before firing in the green state and after firing to meet exacting specifications. Zirconia is electrically conductive above 900°C. Zirconia can be tape cast into very thin sheets for fuel cells and engineered ceramics.
Physical Properties Metric English Comments
Density 5.75 g/cc
0.208 lb/in³
Mechanical Properties Metric English Comments
Knoop Microhardness 1200
1200
kg/mm²
Modulus of Elasticity 200 GPa
29000 ksi
Flexural Strength 620 MPa
89900 psi
Compressive Strength 1750 MPa
254000 psi
Thermal Properties Metric English Comments
CTE, linear 10.1 µm/m-°C

@Temperature 20.0 °C
5.61 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 500 °C
932 °F