Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.152 - 0.208 g/cc | 0.00550 - 0.00752 lb/in³ | Dry |
Reade Advanced Materials Diatomaceous Earth (DE) (SiO2·nH2O) Description: A naturally occurring mineral derived from microscopic in size fossilized remains of marine diatoms. It has high absorption, low bulk density and high brightness.A silica source in the .. |
|||
Density | 0.160 - 0.208 g/cc | 0.00579 - 0.00752 lb/in³ | |
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials |
|||
Density | 0.128 - 0.208 g/cc | 0.00462 - 0.00751 lb/in³ | |
Thermal Ceramics 400 Mineral Fiber Paper 400 grade papers are produced from premium, high quality mineral fibers and organic binders in a unique paper making process. These utility grade papers are noted for their good tensile strengths, o.. |
|||
Density | 0.144 - 0.208 g/cc | 0.00520 - 0.00751 lb/in³ | |
Thermal Ceramics 400-LS Mineral Fiber Paper 400 grade papers are produced from premium, high quality mineral fibers and organic binders in a unique paper making process. These utility grade papers are noted for their good tensile strengths, o.. |
|||
Density | 0.160 - 0.208 g/cc | 0.00578 - 0.00751 lb/in³ | |
Thermal Ceramics Kaowool 2600 Paper Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders in a unique paper making process. Due to its low organic binder content, offgassing is at a minim.. |
|||
Density | 0.176 - 0.208 g/cc | 0.00636 - 0.00751 lb/in³ | |
Thermal Ceramics Kaowool 700 Paper Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders in a unique paper making process. Due to its low organic binder content, offgassing is at a minim.. |
|||
Density | 0.176 - 0.208 g/cc | 0.00636 - 0.00751 lb/in³ | |
Thermal Ceramics Kaowool Flex-Wrap Paper Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders in a unique paper making process. Due to its low organic binder content, offgassing is at a minim.. |
|||
Density | 0.160 - 0.208 g/cc | 0.00578 - 0.00751 lb/in³ | |
Thermal Ceramics Superwool 607 Flex-Wrap Paper Superwool Papers are uniquely designed from Superwool bulk and organic binders in a unique paper making process. Superwool Papers are specially processed to offer excellent performance in high-tempe.. |
|||
Density | 0.160 - 0.208 g/cc | 0.00578 - 0.00751 lb/in³ | |
Thermal Ceramics Superwool 607 Paper Superwool Papers are uniquely designed from Superwool bulk and organic binders in a unique paper making process. Superwool Papers are specially processed to offer excellent performance in high-tempe.. |
|||
Density | 0.128 - 0.208 g/cc | 0.00463 - 0.00752 lb/in³ | |
Monmouth Rubber & Plastics Durafoam™ DK4141 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |