Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.128 g/cc | 0.00463 lb/in³ | Typical Compression Density |
Northstar Polymers MPS-F08A Hand-Mixable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or machine casting by the meter dispensing equipment. The components are stable and liquid at .. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | ASTM D1056 |
Rogers Corporation Bisco® MF1 8055 - 55 Silicone, High Performance Foam, Indentation Force Material MF1® 8055 is a high quality silicone foam material designed for a wide range of cushioning and sealing applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superi.. |
|||
Density | >= 0.128 g/cc | >= 0.00463 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ C42NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ N231XS 100% Neoprene Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Folded |
Unifrax Anchor-Loc® 2200 Ceramic Fiber Modules The Anchor-Loc® module system is a family of ceramic fiber module products designed to meet a wide range of application requirements in a variety of heat processing vessels.Ceramic fiber modules us.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Fibermax mat |
Unifrax Anchor-Loc® 3000 Ceramic Fiber Modules The Anchor-Loc® module system is a family of ceramic fiber module products designed to meet a wide range of application requirements in a variety of heat processing vessels.Ceramic fiber modules us.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Available |
Unifrax Fiberfrax® Durablanket® HP-S Ceramic Fiber Insulator Fiberfrax Durablanket HP-S insulation is a needled blanket made from spun Fiberfrax ceramic fibers. Durablanket HP-S insulation combines all of the physical characteristics offered by Durablanket S.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Edge Grain |
Unifrax Fibermass® 2200 Ceramic Fiber Blocks Fibermass® ceramic fiber blocks combine advancements in fiber chemistry and manufacturing technology to provide an economical lining material for a wide range of heat processing equipment. The Fib.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Unifrax Fibermax® Needled Blanket Fibermax® Needled Blankets are high temperature, light weight and flexible products manufactured from polycrystalline mullite fiber that can be exposed to temperatures up to 1600°C (2912°F). Fib.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Installed Fired |
Unifrax Foamfrax® Grade I Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Installed Fired |
Unifrax Foamfrax® Grade II Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Installed Fired |
Unifrax Foamfrax® Grade III Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Installed Fired |
Unifrax Foamfrax® Isofoam Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Unifrax FyreWrap® 0.5 Plenum Insulation Unifrax's FyreWrap® 0.5 Plenum Insulation is a high-temperature insulation blanket specifically designed to provide a single layer, flexible enclosure around combustible items located within fire-r.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Unifrax FyreWrap® Cable Insulation Unifrax's FyreWrap® Cable Insulation is a thin, flexible, insulation wrap designed to provide a fire-protective enclosure around cable trays and conduit. The FyreWrap system ensures electrical cir.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Unifrax FyreWrap® MAX 2.0 Duct Insulation Two-Layer ASTM E-2336 System Unifrax's FyreWrap® MAX 2.0 Duct Insulation is a high-temperature insulation blanket specifically designed to provide a flexible enclosure for one- and two-hour rated commercial kitchen grease duct.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Module |
Unifrax Insulfrax® 1100C Modules Insulfrax® 1100C Modules are a family of high-temperature module products based on Unifrax's Anchor-Loc® attachment systems. Modules used in the Anchor-Loc® systems are constructed with Insulfra.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 1/8- 8.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Hexcel® HexWeb® HRH-327 - 3/16 - 8.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Hexcel® HexWeb® HRH-78 - 1/8 - 8.0 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Hexcel® HexWeb® HRP - 3/16 - 8.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Hexcel® HexWeb® HRP - 3/8 - 8.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Available |
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator Fiberfrax Durablanket 2600 insulation extends the high-temperature performance of the Durablanket product line. The product is made from high-purity alumina, zirconia, and silica spun ceramic fiber.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Available |
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator Fiberfrax Durablanket S insulation is a strong, lightweight, flexible needled blanket that is made from spun ceramic fibers. Available in a wide variety of thicknesses, widths and densities, Durabl.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | ASTM D1056 |
ACC Magnifoam™ MF1-8055™ MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Density | 0.128 - 0.208 g/cc | 0.00463 - 0.00752 lb/in³ | |
Monmouth Rubber & Plastics Durafoam™ DK4141 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |