Material Notes:
Description: A naturally occurring mineral derived from microscopic in size fossilized remains of marine diatoms. It has high absorption, low bulk density and high brightness.A silica source in the production of calcium silicates, insulation bricks and material in safes, fireproof filing cabinets, etc. Used in the paint, varnish, lacquer, and polish industries. Used as an insecticide in gardens and in swimming pools as a filtering agent.Information provided by Reade Advanced Materials.
Physical Properties Metric English Comments
Specific Gravity 2.00 g/cc
2.00 g/cc
Density 0.152 - 0.208 g/cc
0.00550 - 0.00752 lb/in³
Dry
Loss On Ignition 4.0 %
4.0 %
pH 7.0 - 10
7.0 - 10
10% slurry
Thermal Properties Metric English Comments
Melting Point 1715 °C
3119 °F
Optical Properties Metric English Comments
Refractive Index 1.46
1.46
Descriptive Properties Value Comments
Color off-white to pink