Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.51 g/cc | 0.199 lb/in³ | |
Schott SF57 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 5.51 g/cc | 0.199 lb/in³ | |
Schott SF57HHT Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 5.51 g/cc | 0.199 lb/in³ | |
Schott N-LASF31a Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | >= 5.50 g/cc | >= 0.199 lb/in³ | |
Channel Industries 300 Barium Titanate Piezoelectric Modified barium titanates are widely used in transducers requiring moderate power level and receiving sensitivity. Special characteristics have made barium titanate a proven material for use in devi.. |
|||
Density | 5.50 - 5.60 g/cc | 0.199 - 0.202 lb/in³ | |
Zircar Ceramics MOSI2 Molybdenum Disilicide Heating Element ZIRCAR Molybdenum Disilicide Heating Element Type MOSI2 is an electric element principally containing molybdenum disilicide for use in industrial and laboratory furnaces. Elements fabricated of thi.. |
|||
Density | 5.50 g/cc | 0.199 lb/in³ | |
BASF Sicopal® Yellow L 1100 Color Additive Description: Weather-resistant inorganic bismuth vanadate pigment with high hiding powerChemical Structure: Bismuth vanadatSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems,.. |