Polymer Property : Density = 5.50 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density >= 5.50 g/cc
>= 0.199 lb/in³
Channel Industries 300 Barium Titanate Piezoelectric
Modified barium titanates are widely used in transducers requiring moderate power level and receiving sensitivity. Special characteristics have made barium titanate a proven material for use in devi..
Density 5.50 - 5.60 g/cc
0.199 - 0.202 lb/in³
Zircar Ceramics MOSI2 Molybdenum Disilicide Heating Element
ZIRCAR Molybdenum Disilicide Heating Element Type MOSI2 is an electric element principally containing molybdenum disilicide for use in industrial and laboratory furnaces. Elements fabricated of thi..
Density 5.50 g/cc
0.199 lb/in³
BASF Sicopal® Yellow L 1100 Color Additive
Description: Weather-resistant inorganic bismuth vanadate pigment with high hiding powerChemical Structure: Bismuth vanadatSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems,..