Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.51 g/cc | 0.199 lb/in³ | |
Schott SF57 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 5.51 g/cc | 0.199 lb/in³ | |
Schott SF57HHT Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 5.51 g/cc | 0.199 lb/in³ | |
Schott N-LASF31a Glass Information Provided by SCHOTT North America, Inc. |