Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.79 g/cc | 0.173 lb/in³ | |
MarkeTech Indium Phosphide Semiconductor Wafer, n-type, Sulfur + Tin Doped, Czochralski-LEC Grown Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of .. |
|||
Density | 4.79 g/cc | 0.173 lb/in³ | |
MarkeTech Indium Phosphide Semiconductor Wafer, p-type, Zinc Doped, Czochralski-LEC Grown Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of .. |
|||
Density | 4.79 g/cc | 0.173 lb/in³ | |
MarkeTech Indium Phosphide Semiconductor Wafer, Semi-Insulating Iron Doped, Czochralski-LEC Grown Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of .. |
|||
Density | 4.80 - 5.80 g/cc | 0.173 - 0.210 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 559.074 Agglomerated, Sintered Tungsten Carbide-Cobalt-Chromium 86-6-8 (WC-Co-Cr) |
|||
Density | 4.79 g/cc | 0.173 lb/in³ | |
Schott SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.78 g/cc | 0.173 lb/in³ | Typical |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Density | 4.78 g/cc | 0.173 lb/in³ | Typical |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 482°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Density | 4.78 g/cc | 0.173 lb/in³ | Typical |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Density | 4.78 g/cc | 0.173 lb/in³ | apparent |
Wall Colmonoy COLMONOY® 88 Hard-Surfacing Alloy Description: Colmonoy 88 is a unique alloy containing fine, multiple hard phases which are uniformly distributed throughout a Ni-Cr-B matrix. These hard phases, comprised of complex bi- and tri-met.. |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 g/cc | 0.173 lb/in³ | |
BASF Sicotan® Brown K 2711 Color Additive Chemical Structure: Mn/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ | |
Alliance C-8B Strontium Ferrite Ceramic Magnetic Material |
|||
Density | 4.80 g/cc | 0.173 lb/in³ | A Component; ASTM D1475 |
Aptek 6516-A/B Electrically conductive epoxy adhesive General purpose, electrically conductive epoxy adhesiveAPTEK 6516-A/B is a two component, 100% solid, silver filled electrically conductive epoxy adhesive specifically designed for the attachment of.. |
|||
Density | 4.80 g/cc | 0.173 lb/in³ | B Component; ASTM D1475 |
Aptek 6516-A/B Electrically conductive epoxy adhesive General purpose, electrically conductive epoxy adhesiveAPTEK 6516-A/B is a two component, 100% solid, silver filled electrically conductive epoxy adhesive specifically designed for the attachment of.. |