Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.79 g/cc | 0.173 lb/in³ | |
MarkeTech Indium Phosphide Semiconductor Wafer, n-type, Sulfur + Tin Doped, Czochralski-LEC Grown Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of .. |
|||
Density | 4.79 g/cc | 0.173 lb/in³ | |
MarkeTech Indium Phosphide Semiconductor Wafer, p-type, Zinc Doped, Czochralski-LEC Grown Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of .. |
|||
Density | 4.79 g/cc | 0.173 lb/in³ | |
MarkeTech Indium Phosphide Semiconductor Wafer, Semi-Insulating Iron Doped, Czochralski-LEC Grown Data provided by the supplier, MarkeTech International.These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: ±20' or 2-3° of .. |
|||
Density | 4.79 g/cc | 0.173 lb/in³ | |
Schott SF4 Glass Information Provided by SCHOTT North America, Inc. |