Polymer Property : Density = 0.170 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.170 g/cc
0.00614 lb/in³
Mo-Sci Corporation GL-0193 Hollow Glass Spheres
Appearance: Hollow microspheres with white color in powder form.Applications: GL-0193 is a new, low cost, light weight, hollow glass extender for liquid resin systems offering low cost per unit volu..
Density 0.170 g/cc
0.00614 lb/in³
Pour Density; ASTM D1513
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Density 0.170 g/cc
0.00614 lb/in³
Pour Density; ASTM D1513
TIMCAL ENSACO™ 260G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..