Mo-Sci Corporation GL-0193 Hollow Glass Spheres

Category Ceramic , Glass
Manufacturer Mo-Sci Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mo-Sci Corporation GL-0193 Hollow Glass Spheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appearance: Hollow microspheres with white color in powder form.Applications: GL-0193 is a new, low cost, light weight, hollow glass extender for liquid resin systems offering low cost per unit volume displacement. Since GL-0193 displaces 8 to 10 times its weight of conventional mineral fillers, it will reduce the weight and, therefore, the cost of most products. Parts produced with GL-0193 exhibit excellent staple, screw and nail holding power. The low thermal conductivity of GL-0193 also provides excellent thermal insulation for coating systems.Information provided by Mo-Sci Corporation.
Physical Properties Metric English Comments
Bulk Density 0.120 g/cc
0.00434 lb/in³
of Dry Beads
Density 0.170 g/cc
0.00614 lb/in³
pH 7.2
7.2
in water
Mechanical Properties Metric English Comments
Compressive Strength 8.48 MPa
1230 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.0519 W/m-K
0.360 BTU-in/hr-ft²-°F
Softening Point 980 °C
1800 °F