Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TIMCAL ENSACO™ 260G Conductive Carbon Black

Category Carbon , Carbon Black , Other Engineering Material , Additive/Filler for Polymer
Manufacturer TIMCAL
Trade Name ENSACO™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMCAL ENSACO™ 260G Conductive Carbon Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can originate from the interstices between the carbon black particle due to their complex arrangement and from the porosity.Applications:black pigmentUV stabilizerrubber reinforcementInformation provided by TIMCAL
Physical Properties Metric English Comments
Density 0.170 g/cc
0.00614 lb/in³
Pour Density; ASTM D1513
Volatiles <= 0.20 %
<= 0.20 %
Weight loss during heating between 105 and 950°C; Internal Method 02
Oil Absorption 190 %
190 %
OAN (Oil Absorption Number) ml/100g; ASTM D2414
Particle Size 45 µm
45 µm
2 ppm sieve residue; ASTM D1514
pH 8.0 - 11
8.0 - 11
ASTM D1512
Specific Surface Area 70 m²/g
70 m²/g
BET Nitrogen Surface Area; ASTM D3037
Ash 0.010 %
0.010 %
ASTM D1506
Component Elements Properties Metric English Comments
Sulfur, S 0.020 %
0.020 %
ASTM D1619
Electrical Properties Metric English Comments
Volume Resistivity 8.0 ohm-cm
8.0 ohm-cm
25% Carbon Black
100 ohm-cm
100 ohm-cm
18% Carbon Black
1000 ohm-cm
1000 ohm-cm
15% Carbon Black
10000 ohm-cm
10000 ohm-cm
14% Carbon Black
3.25 ohm-cm

@Time 300 sec
3.25 ohm-cm

@Time 0.0833 hour
25% Carbon Black
3.5 ohm-cm

@Time 420 sec
3.5 ohm-cm

@Time 0.117 hour
25% Carbon Black
4.0 ohm-cm

@Time 540 sec
4.0 ohm-cm

@Time 0.150 hour
25% Carbon Black
50 ohm-cm

@Time 300 sec
50 ohm-cm

@Time 0.0833 hour
18% Carbon Black
75 ohm-cm

@Time 540 sec
75 ohm-cm

@Time 0.150 hour
18% Carbon Black
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
as packed; ASTM D1509
Descriptive Properties Value Comments
Aspect Fine black granules
COAN (Crushed OAN) ml/100g 104
ASTM D3493
Toluene Extract, Max, % 0.1
ASTM D4527
Users viewing this material also viewed the following: