Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.22 g/cc | 0.152 lb/in³ | |
MarkeTech Yttrium Vanadate (YVO4) Fiber Optic Crystal Large birefringence and wide transparency range (400 to 4000 nm); finds uses as fiber optic isolators, circulators, and beam displacers. Grown by Czochralski method.Data provided by the supplier, M.. |
|||
Density | 4.20 g/cc | 0.152 lb/in³ | |
Mo-Sci Corporation GL-0176 Barium-Titanate Glass Spheres Appearance: Solid glass microspheres with light yellow color in powder form.Typical applications of GL0176 beads include: high temperature spacer material for gauge control, coating, filler for plas.. |
|||
Density | 4.20 - 4.50 g/cc | 0.152 - 0.163 lb/in³ | |
Mo-Sci Corporation GL-0275-B Class VI Barium-Titanate Glass Spheres Appearance: Solid glass microspheres with light yellow color in powder form.Typical applications of GL0275-B beads including: high temperature spacer material for gauge control, coating, filler for .. |
|||
Density | 4.20 g/cc | 0.152 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT 4.2 specific gravity, PBT, gray |
|||
Density | 4.20 g/cc | 0.152 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT 4.2 specific gravity, PBT, gray |
|||
Density | 4.22 g/cc | 0.152 lb/in³ | |
Schott N-LAK33A Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.20 g/cc | 0.152 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® C429-2 One-Component Silver Filled Electrically Conductive Epoxy Adhesive Emerson & Cuming C429-2 Eccobond® One-Component Silver Filled Electrically Conductive Epoxy AdhesiveOne component, high strength, moderate cost, silver filled, electrically conductive, epoxy adhesi.. |
|||
Density | 4.20 g/cc | 0.152 lb/in³ | |
CeramTec 965 Toughened Alumina (Al2O3-ZrO2) Hasselman Thermal Shock value is 270 K.Data provided by CeramTec North America. |
|||
Density | 4.20 - 4.50 g/cc | 0.152 - 0.163 lb/in³ | |
Mo-Sci Corporation GL-0175 Barium-Titanate Glass Spheres Appearance: Solid glass microspheres with light yellow color in powder form.Typical applications of GL0175 beads include:: high temperature spacer material for gauge control, coating, filler for pla.. |