Trelleborg Emerson & Cuming Eccobond® C429-2 One-Component Silver Filled Electrically Conductive Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® C429-2 One-Component Silver Filled Electrically Conductive Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming C429-2 Eccobond® One-Component Silver Filled Electrically Conductive Epoxy AdhesiveOne component, high strength, moderate cost, silver filled, electrically conductive, epoxy adhesive. Excellent adhesion and long term durability. Designed for use in miniature lamp bonding. Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 4.20 g/cc
0.152 lb/in³
Viscosity 2.50e+6 cP

@Temperature 25.0 °C
2.50e+6 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Adhesive Bond Strength 13.8 MPa
2000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.20 ohm-cm
0.20 ohm-cm
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 180 °C
0.0833 hour

@Temperature 356 °F
30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
90.0 min

@Temperature 125 °C
1.50 hour

@Temperature 257 °F
Descriptive Properties Value Comments
Color Silver