Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.144 g/cc | 0.00521 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Density | 0.144 g/cc | 0.00521 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent.. |
|||
Density | 0.144 g/cc | 0.00521 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Density | 0.144 g/cc | 0.00521 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Density | 0.144 g/cc | 0.00521 lb/in³ | Compressed Density |
Northstar Polymers MPP-M09D "Slow Cure" Semi-Rigid Foam Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is set longer than ordinary rigid foam formulatio.. |
|||
Density | 0.144 g/cc | 0.00520 lb/in³ | |
Pyrotek M-9 Fiberseal Blanket Maxsil ceramic-free insulation with excellent chemical resistance. Shot free.Dimensions889 mm x 24.4 m x 13 mm889 mm x 11.9 m x 25 mmApplicationsBlankets Information provided by Pyrotek. |
|||
Density | 0.144 - 0.176 g/cc | 0.00521 - 0.00637 lb/in³ | |
Mid-Mountain Materials CERMEX® MT1000 Needled Fiberglass Mat CERMEX® MT1000 fiberglass mat is comprised of high purity, highly resilient E-Glass fibers. CERMEX® MT1000 is lightweight, strong, and highly efficient as insulation in most high heat environm.. |
|||
Density | 0.144 - 0.272 g/cc | 0.00521 - 0.00984 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK5151 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.144 g/cc | 0.00521 lb/in³ | |
Mid-Mountain Materials CERMEX® MT1200 Thermal Insulation Mat CERMEX MT1200 is a non-woven insulation mat for use in high temperature applications up to 1600°F (871°C). The fibers are mechanically bonded and contain no additional resins or adhesives. T.. |
|||
Density | 0.144 g/cc | 0.00520 lb/in³ | ASTM D1667 |
Saint-Gobain Norton® V740 Multipurpose Pressure Sensitive Adhesive Sealant Foam Description: Medium Density, Multipurpose Foam: Norseal V740 is a closed-cell polyvinyl chloride foam sealant with pressure-sensitive adhesive on one side designed to provide an economical solution .. |
|||
Density | 0.144 g/cc | 0.00520 lb/in³ | ASTM D1667 |
Saint-Gobain Norton® V780 Medium-Density Pressure Sensitive Adhesive Sealant Foam Description: Improved Performance: Norseal® V780 medium density foam sealant combines a closed cell foam substrate with a one-sided pressure-sensitive adhesive. Norseal has been specially formula.. |
|||
Density | 0.144 - 0.160 g/cc | 0.00521 - 0.00579 lb/in³ | |
Unifrax Insulfrax® Paper Insulfrax® Paper is an evolutionary product which is manufactured by forming Insulfrax Fiber in a nonwoven matrix. These fibers are randomly oriented during manufacturing and then held in place wi.. |
|||
Density | 0.144 - 0.208 g/cc | 0.00520 - 0.00751 lb/in³ | |
Thermal Ceramics 400-LS Mineral Fiber Paper 400 grade papers are produced from premium, high quality mineral fibers and organic binders in a unique paper making process. These utility grade papers are noted for their good tensile strengths, o.. |
|||
Density | 0.144 g/cc | 0.00520 lb/in³ | |
Thermal Ceramics Unifelt 3000XT Unifelt Veneering modules, 3000 (HT), 3000 M, XT are made from a blend of high-temperature Kaowool fiber and Saffil alumina fiber. The modules are fabricated into blocks, 12" by 12" (305 mm x 305 mm.. |
|||
Density | 0.144 g/cc | 0.00521 lb/in³ | |
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Density | 0.144 g/cc | 0.00521 lb/in³ | |
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Density | 0.144 g/cc | 0.00521 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 1/8- 9.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.144 g/cc | 0.00520 lb/in³ | Molded density, ASTM D3574-A |
Covestro Bayfill® 361 Polyurethane Semi-Rigid Foam, Conventional Catalyst, Open Pour, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 0.144 - 0.184 g/cc | 0.00521 - 0.00666 lb/in³ | Range represents a tolerance from nominal of -10%/+15%.; ISO 845 |
DIAB Klegecell® R 200 Rigid, Closed Cell PVC Foam Core Material Klegecell R is a PVC based, rigid, closed-cell foam with a tri-dimensional grid structure, which provides high thermal stability and structural integrity. As a structural core, Klegecell R is used i.. |
|||
Density | 0.144 - 0.192 g/cc | 0.00521 - 0.00694 lb/in³ | Range represents a tolerance from nominal of -10%/+20%; ASTM D1622 |
DIAB TBR® 10 Multifunctional Polymer Core Material TBR® is a multifunctional polymer core designed for hard points within sandwich structures where through-bolting or point-loading would normally cause local crushing of low density sandwich cores. .. |
|||
Density | 0.144 g/cc | 0.00520 lb/in³ | |
Thermal Ceramics Kaomat Blanket Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets... |
|||
Density | 0.144 - 0.160 g/cc | 0.00520 - 0.00578 lb/in³ | |
Thermal Ceramics Kaomat SL Blanket Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets... |