Polymer Property : Density = 0.00521 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.144 g/cc
0.00521 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
Density 0.144 g/cc
0.00521 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced
Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent..
Density 0.144 g/cc
0.00521 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Density 0.144 g/cc
0.00521 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Density 0.144 g/cc
0.00521 lb/in³
Compressed Density
Northstar Polymers MPP-M09D "Slow Cure" Semi-Rigid Foam Formulation
This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is set longer than ordinary rigid foam formulatio..
Density 0.144 - 0.176 g/cc
0.00521 - 0.00637 lb/in³
Mid-Mountain Materials CERMEX® MT1000 Needled Fiberglass Mat
CERMEX® MT1000 fiberglass mat is comprised of high purity, highly resilient E-Glass fibers. CERMEX® MT1000 is lightweight, strong, and highly efficient as insulation in most high heat environm..
Density 0.144 - 0.272 g/cc
0.00521 - 0.00984 lb/in³
Monmouth Rubber & Plastics Durafoamâ„¢ DK5151 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Density 0.144 g/cc
0.00521 lb/in³
Mid-Mountain Materials CERMEX® MT1200 Thermal Insulation Mat
CERMEX MT1200 is a non-woven insulation mat for use in high temperature applications up to 1600°F (871°C). The fibers are mechanically bonded and contain no additional resins or adhesives. T..
Density 0.144 - 0.160 g/cc
0.00521 - 0.00579 lb/in³
Unifrax Insulfrax® Paper
Insulfrax® Paper is an evolutionary product which is manufactured by forming Insulfrax Fiber in a nonwoven matrix. These fibers are randomly oriented during manufacturing and then held in place wi..
Density 0.144 g/cc
0.00521 lb/in³
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..
Density 0.144 g/cc
0.00521 lb/in³
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..
Density 0.144 g/cc
0.00521 lb/in³
Hexcel® HexWeb® HRH-10 - 1/8- 9.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Density 0.144 - 0.184 g/cc
0.00521 - 0.00666 lb/in³
Range represents a tolerance from nominal of -10%/+15%.; ISO 845
DIAB Klegecell® R 200 Rigid, Closed Cell PVC Foam Core Material
Klegecell R is a PVC based, rigid, closed-cell foam with a tri-dimensional grid structure, which provides high thermal stability and structural integrity. As a structural core, Klegecell R is used i..
Density 0.144 - 0.192 g/cc
0.00521 - 0.00694 lb/in³
Range represents a tolerance from nominal of -10%/+20%; ASTM D1622
DIAB TBR® 10 Multifunctional Polymer Core Material
TBR® is a multifunctional polymer core designed for hard points within sandwich structures where through-bolting or point-loading would normally cause local crushing of low density sandwich cores. ..