Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.75 - 3.80 g/cc | 0.135 - 0.137 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9622 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.75 - 3.80 g/cc | 0.135 - 0.137 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9634 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | >= 3.75 g/cc | >= 0.135 lb/in³ | |
MarkeTech AO 98 Aluminum Oxide Ceramic Substrate, 98% Purity Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 4.0 x 6.0 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 Â.. |
|||
Density | 3.75 g/cc | 0.135 lb/in³ | |
Schott N-BAF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.74 g/cc | 0.135 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM CO 0374 S Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Density | 3.73 g/cc | 0.135 lb/in³ | |
Schott N-LAF7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.74 g/cc | 0.135 lb/in³ | |
Schott N-LAK21 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.75 g/cc | 0.135 lb/in³ | |
Schott N-LAK8 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.75 g/cc | 0.135 lb/in³ | |
CeramTec Rubalit® 708 Alumina, 96% Based on 96% aluminum oxide, Rubalit® 708 was developed specifically for making heavy-duty resistors and miniature metal layer resistors. Because of its outstanding strength, this same material is .. |
|||
Density | 3.73 g/cc | 0.135 lb/in³ | DIN EN 623-2 |
CeramTec Rubalit® IS 95 Alumina Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva.. |
|||
Density | 3.75 g/cc | 0.135 lb/in³ | DIN EN 623-2 |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Density | 3.75 g/cc | 0.135 lb/in³ | ASTM-C373 |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
Density | 3.75 g/cc | 0.135 lb/in³ | ASTM-C373 |
CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film Applications: thick films and lasers |
|||
Density | 3.73 g/cc | 0.135 lb/in³ | DIN EN 623-2 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |