Polymer Property : Density = 3.73 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 3.73 g/cc
0.135 lb/in³
Schott N-LAF7 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.73 g/cc
0.135 lb/in³
DIN EN 623-2
CeramTec Rubalit® IS 95 Alumina
Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva..
Density 3.73 g/cc
0.135 lb/in³
DIN EN 623-2
CeramTec Rubalit® A 1896 Alumina
Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele..