Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.67 g/cc | 0.0965 lb/in³ | |
Schott BG40 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Density | 2.67 g/cc @Temperature 25.0 °C |
0.0965 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8240 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, free from alkali, blue colored, defined absorption Bulb and exhaust tube .. |
|||
Density | 2.67 g/cc @Temperature 25.0 °C |
0.0965 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8253 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, for use at higher temperatures than glass 8252, free from alkali Bulb and.. |
|||
Density | 2.67 g/cc @Temperature 25.0 °C |
0.0965 lb/in³ @Temperature 77.0 °F |
|
Schott NEO 1730 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature applications in electrical engineering, for sealing to molybdenum, free from alkali Bulb and exhaust tube for halogen lamps for automotive,.. |
|||
Density | 2.67 g/cc @Temperature 17.0 °C |
0.0965 lb/in³ @Temperature 62.6 °F |
|
Solvay Chemicals NOCOLOK® CB Flux Potassium Silicofluoride Reactive flux for brazing of aluminumCAS-No.: 16871-90-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided .. |
|||
Density | 2.67 g/cc | 0.0965 lb/in³ | |
Constellium PLAN 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Density | 2.67 g/cc | 0.0965 lb/in³ | |
Constellium PLAN OX 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone.. |
|||
Density | 2.67 g/cc @Temperature 25.0 °C |
0.0965 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8241 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, free from alkali, blue colored, defined absorption Bulb and exhaust tube .. |