Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.67 g/cc
0.0965 lb/in³
Thermal Properties Metric English Comments
CTE, linear 11.9 µm/m-°C

@Temperature -30.0 - 70.0 °C
6.61 µin/in-°F

@Temperature -22.0 - 158 °F
13.7 µm/m-°C

@Temperature 20.0 - 300 °C
7.61 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 305 °C
581 °F
Optical Properties Metric English Comments
Refractive Index 1.53

@Wavelength 587.6 nm
1.53

@Wavelength 587.6 nm
He
1.54

@Wavelength 404.7 nm
1.54

@Wavelength 404.7 nm
Hg
Transmission, Visible 15 %

@Wavelength 690 nm
15 %

@Wavelength 690 nm
90 %

@Wavelength 450 - 530 nm
90 %

@Wavelength 450 - 530 nm
Internal transmittance of 98% at 450-530 nm
IR Transmittance 75 %

@Wavelength 2100 nm
75 %

@Wavelength 2100 nm
Internal transmittance of 81% at 2100 nm.
UV Transmittance <= 2.0 %

@Wavelength 200 - 310 nm
<= 2.0 %

@Wavelength 200 - 310 nm
88 %

@Wavelength 390 nm
88 %

@Wavelength 390 nm
Internal transmittance of 95% at 390 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 5.1
5.1
Alkali Class, AR 3
3
Stain Resistance Class, FR 0.0
0.0
Users viewing this material also viewed the following: