Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.880 - 2.40 g/cc | 0.0318 - 0.0867 lb/in³ | Average value: 0.935 g/cc Grade Count:752 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Density | 2.20 - 2.40 g/cc | 0.0795 - 0.0867 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 827.6 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 - 2.40 g/cc | 0.0795 - 0.0867 lb/in³ | |
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |