Polymer Property : Density = 0.0741 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.05 g/cc
0.0741 lb/in³
Green Density
Nabaltec NABALOX® NO 313 Ground Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 2.05 - 2.15 g/cc
0.0741 - 0.0777 lb/in³
ASTM D792
Polikim EFALON® K-25 PTFE, 25% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...
Density 2.05 g/cc
0.0741 lb/in³
Cookson Group Plaskon® 435 Mineral Filled Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.Combines exceptional reliability with wide molding process latitude. This material is designed to encapsulate a variety of semic..
Density 2.05 g/cc
0.0741 lb/in³
ASTM D792
Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound  (discontinued **)
Black Polyphenylene Sulfide CompoundRyton® R10-110BL is a glass and mineral filled polyphenylene sulfide compound which provides a good combination of mechanical and electrical properties.Applicati..
Density 2.05 g/cc
0.0741 lb/in³
estimated by MatWeb
Garlock GYLON® 3540 Microcellular PTFE Gasketing
Microcellular PTFE.Highly compressible PTFE seals under low bolt load- suitable for many non-metallic flangesCompressible material conforms to surface irregularities, especially on warped, pitted or..
Density 2.05 g/cc
0.0741 lb/in³
estimated by MatWeb
Garlock GYLON® 3545 Layered Microcellular PTFE Gasketing
Microcellular PTFE gasket with rigid PTFE coreHighly compressible PTFE outer layers seal under low bolt load- suitable for many non-metallic flangesCompressible layers conform to surface irregularit..
Density 2.05 - 2.11 g/cc
0.0741 - 0.0762 lb/in³
molded; ASTM D792
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Density 2.05 - 2.11 g/cc
0.0741 - 0.0762 lb/in³
molded; ASTM D792
Guarniflon PTFE G456 Polytetrafluoroethylene 25% Hard Carbon
PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w..
Density 2.05 g/cc

@Temperature 77.9 °C
0.0741 lb/in³

@Temperature 172 °F
Liquid at mp
Indium Corp. GaCl3 Gallium Trichloride, Anhydrous
Synonyms: Gallium Chloride, Gallium (III) ChlorideCAS Number: 13450-90-3EC Number: 236-610-0RTECS: LW9100000Purity: 99.5 to 99.999% Gallium TrichlorideAppearance: Clear or White, Needle-shaped..
Density 2.05 - 2.11 g/cc
0.0741 - 0.0762 lb/in³
molded; ASTM D792
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Density 2.05 - 2.13 g/cc
0.0741 - 0.0770 lb/in³
BS2782:Pt6
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..
Density 2.05 g/cc
0.0741 lb/in³
Trelleborg Emerson & Cuming Stycast® 5952 Two-Component Easy Mix Ratio Encapsulant
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, ..
Density 2.05 - 2.13 g/cc
0.0741 - 0.0770 lb/in³
BS2782:Pt6
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..
Density 2.05 g/cc
0.0741 lb/in³
BNZ Materials Blazecrete 2800 Dense Castable
Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur..
Density 2.05 g/cc
0.0741 lb/in³
ASTM D792 Method A
Arlon 91ML Low-Cost Halogen-Free Thermally Conductive Epoxy
Thermally conductive, multilayerable laminate and prepreg circuit board material. Available in various resin content percentages.Arlon 91ML ceramic filled thermally conductive multifunctional epoxy..
Density 2.05 - 2.15 g/cc
0.0741 - 0.0777 lb/in³
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 2.05 g/cc
0.0741 lb/in³
LATI Latimass 52/11-01 D020 PP Homopolymer
Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..