Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0550 g/cc | 0.00199 lb/in³ | Molded density, ASTM D1622 |
Covestro Bayfill® EA 4004 Polyurethane Energy-Absorbing Semi-Rigid Foam, Rigid Grade, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 0.0550 - 0.0650 g/cc | 0.00199 - 0.00235 lb/in³ | |
Akzo Nobel Expancel® 051 DE 40 d60 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0550 - 0.0650 g/cc | 0.00199 - 0.00235 lb/in³ | |
Akzo Nobel Expancel® 461 DE 40 d60 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0550 - 0.0650 g/cc | 0.00199 - 0.00235 lb/in³ | |
Akzo Nobel Expancel® 551 DE 20 d60 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |