SGL Carbon Group PANOX® FA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer SGL Carbon Group
Trade Name PANOX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group PANOX® FA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For carbon/carbon and spinning. PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX is ideal for processing into yarns, woven fabrics, nonwovens and felts.Information provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
Fiber Density
Filament Diameter 13 µm
13 µm
Fiber Count 1.67 dtex
1.50 denier
Mechanical Properties Metric English Comments
Tensile Strength at Break 190 MPa
27600 psi
Elongation at Break 15 - 27 %
15 - 27 %
Tenacity >= 0.140 N/tex
>= 1.59 g/denier
Descriptive Properties Value Comments
Typical Finish Content, % 0.6